Tool Steel

Perfect for high temperature, high wear applications.

Heat to Harden

Tool Steel gets harder, stronger, and tougher when heat treated. We recommend air quenching at 1010C (1850F) and double tempering at 600C (1110F). For improved hardness at the expense of part toughness, you can double temper at a lower temperature (500-550C, 930–1022F).

Order Now
humidity

Resolution Supported

100 Micron – 0.1 mm

resilience

Max Part Size

235 x 68.3 x 75 mm

pipette

Available Colors

  • Steel

Material Properties

Strength
Stiffness
Heat Tolerance
Cost
Properties Sintered Wrought Heat Treated
0.2% Compressive Yield Strength 900 MPa
Elastic Modulus 180 GPa 190 GPa
Hardness 52 HRC 63 HRC
Relative Density > 94.5% 100%
Material Data Sheet